What causes major slag inclusion/ porous welds when all other welds went fine?
Welding indoors and all bare/ new metal
Welding indoors and all bare/ new metal
Faulty/sticking gas solenoid?It was mig and the steel was prepared the same for all 4 welds. 3 went perfectly but one wouldnt stop going porous like i turned the gas off.
2 of the good welds were done after the bad one.
Ive had this happen a few times with this welder hence the question.
Not me I'm afraidIs a cartoon character kinking your shielding gas hose as soon as you flip your hood down?
too high in a draft free environment ... 10 is more than adequate ... you'll chill the weld with too high a pressure .... also as Mike said diffusers and shrouds play a big role in a complete gas shield around the weld .. even the tip if not kept clean and in the shape it arrives in new. Optimum set up is the key to a perfect weld ... MIG or stick or even gas.I've only got a dial guage not a floating ball type ( been told there not as good) but it was 15 psi now 20 I think. I will check the tip and nozzle.![]()
I've included plenty of slags in things over the years... no longer, however!![]()